I noticed on my Curt Tuning Point pin box that is 5 months old, that the washers are corroding. I’m wire brushing the rust in order to paint, but if this is dissimilar metals corrosion, it will continue unless the washers are replaced or something else is changed.
Has anyone else run into this issue? Any suggestions?